DX SHACKLE

DX Shackle    J&L

  • Working load T8 grade: 2t-110t; S6 grade : 0.5t-85t
  • T8 grade is high quality structural alloy steel; S6 grade is structural alloy steel
  • The maximum testing load is 2 times of working load, the minimum breaking load is 4 times of working load
  • About the bearing capacity of 2t-80t, T8 grade is 40%-100% up higher then the S6 grade in the same dimension
  • About the bearing capacity of 110t, T8 grade is 29% up higher than the S6 grade in the same dimension
  • The products in accordance with the technical requirements and testing methods of ISO2415-2004